How to specify FRP grating on drawings: generic callout guide

A surprising number of FRP grating submittals get rejected for one reason: the drawing callout was not written as a specification. “FRP GRG, 38 MM” on a plan tells the fabricator the depth and nothing else — not the mesh opening, not the bar construction, not the resin, not the span the panels were sized for. Every one of those gaps becomes a change order, a wrongly substituted panel, or a walkway that feels like a trampoline. The Eng-Tips threads on this topic keep circling the same question: what exactly should the callout say so any qualified manufacturer can bid, and the delivered panel still meets the design intent? This guide gives the four elements that must appear, the numbers that make them enforceable, and a worked generic callout you can paste onto your next plan set.

Why generic, performance-based callouts win

Naming one manufacturer’s part number on the drawing feels safe but creates three problems: procurement cannot get competing bids, a long-lead item stalls the schedule, and a substitution request arrives after award with different load data. The alternative — a generic callout that states performance and configuration, not brand — lets two or three FRP grating suppliers bid against each other while the engineer keeps control of the engineering requirements. The trick is that a generic callout only works if it is complete. A brand-name callout inherits all the properties of the product; a generic callout has to state each property explicitly.

The four elements every FRP grating callout must state

Depth, mesh spacing, bar thickness, and resin system. Miss any one of the four and the specification is incomplete.

  1. Panel depth. The primary stiffness driver. Common pultruded and molded FRP grating depths run 25 mm, 30 mm, 38 mm, 40 mm and 50 mm. Panel stiffness scales roughly with the cube of depth, so a 38 mm panel is not “a bit” stiffer than a 25 mm panel — deflection under the same load and span drops by well over half. Depth is chosen from the load table against the span, never guessed.
  2. Mesh opening (bar spacing). The clear opening between bearing bars. The workhorse configuration is 38 × 38 mm square mesh; denser 19 × 19 mm or 12 × 12 mm “micro mesh” is used where small tools, heel capture, or bird control matter; 25 × 100 mm rectangular mesh is the accessibility pattern for wheelchair traffic on public walkways (opening elongated in the walking direction). The opening also sets open area, which governs drainage, snow shedding, and whether the grating meets the 13 mm sphere rule common in water treatment plant specs (openings ≤ 13 mm in areas with public access, per typical municipal standards).
  3. Bar thickness and construction. State both the bearing bar thickness and whether the grating is pultruded I-bar, pultruded rectangular/T-bar, or molded. Pultruded I-bars (typically ~6.4 mm web with flanges) deliver the best stiffness-to-weight; rectangular pultruded bars are heavier but tolerate point loads and curb edges better; molded grating (interleaved glass strands, no distinct bars) is isotropic — it can be cut without losing one-way strength, which matters for odd-shaped panels and openings. The callout must say which, because a load table for one does not apply to another at the same depth.
  4. Resin system. This is the element most often missing, and it is the one that decides service life in any corrosive or outdoor environment. The standard ladder: orthophthalic polyester (economy, indoor, non-chemical), isophthalic polyester (the default corrosion grade — wastewater, coastal, general chemical), vinyl ester (severe chemical service, acids and solvents, longest service life), phenolic (fire-critical and offshore — low smoke and flame, DNV-type offshore specs). If the drawing says nothing, a bidder is entitled to quote the cheapest resin that matches the visible product — and in a chlorinated wastewater atmosphere an orthophthalic panel can show visible resin erosion in a few years. Final resin selection must be confirmed against the manufacturer’s chemical-resistance data for the actual service (chemical, concentration, temperature).

Surface, fire and slip: completing the callout

Three more attributes complete a defensible specification:

  • Top surface: meniscus (smooth concave, standard) vs grit-top (embedded angular grit for wet/oily service). For hydrotesting decks, offshore walkways and any wet process area, grit-top is the default; slip performance is specified as grit top with supplier test data under a current project-accepted method (e.g. DIN 51130 R-rating) — ASTM C1028 has been withdrawn — which is what the safety reviewer will ask for.
  • Fire rating: tested to ASTM E84 with flame-spread index ≤ 25 (Class 1/A) is the standard requirement for building interiors; phenolic or specially formulated polyester systems achieve it — require the panel’s test report, not just the class label. UK and international projects typically reference BS 476 Part 7 Class 1 or EN 13501 classifications instead — match the callout to the jurisdiction.
  • UV and veil: outdoor installations need UV inhibitor in the resin and a synthetic surface veil for corrosion barrier retention; state “UV stabilized” explicitly for exterior work.

Load, span and deflection: making the numbers enforceable

A grating load is meaningless without a span, and both belong on the drawing. The enforceable statement has three parts:

  1. Design live load. Industrial walkway platforms are commonly designed for a uniformly distributed load of 4.8 kPa (100 psf); access platforms and stair treads for a concentrated load case (typically a 4.5 kN load on a 300 mm square footprint, or per local code) — state which governs, or both.
  2. Support span. The clear span between bearing supports. Fibergrate guidance: 914–1,067 mm typical for 38 mm molded grating at 2.4–3.1 kPa pedestrian load, deflection ≤ the lesser of L/120 or 9.5 mm; 51 mm reaches 1,219–1,372 mm. Depth alone never sets span — verify against the specific manufacturer’s load table. State it center-to-center of bearers on the plan.
  3. Deflection limit. The accepted industry limit for pedestrian FRP grating is L/200 under design live load (some manufacturers allow L/150 for utility access). Writing “deflection limited to L/200 under 4.8 kPa live load over the stated span” converts the depth choice from a suggestion into a checkable requirement — the submittal must include load-deflection test data demonstrating it.

The submittal requirement closes the loop: require the manufacturer to submit published load tables and panel test data (flexural coupon testing per ASTM D790 plus full-panel proof load results) demonstrating the deflection limit at the stated span. A supplier who cannot produce panel-level data for the exact depth and mesh quoted has not met the spec.

A worked generic callout

Assemble the elements into one line that fits a drawing bubble:

FRP GRATING, PULTRUDED I-BAR, 38×38 MESH, 38 DEEP, ISO RESIN, GRIT TOP, ASTM E84 CLASS 1, UDL 4.8 kPa @ 1200 SPAN, Δ ≤ L/200, UV STABILIZED

Callout tokenWhat it fixesWhy it matters
PULTRUDED I-BARProcess and bar constructionLoad tables differ between pultruded and molded
38×38 MESHClear openingDrainage and open area; go denser (19×19 / 12×12) where heel capture or the 13 mm sphere rule applies
38 DEEPStiffness driverSets achievable span and deflection
ISO RESINCorrosion classIsophthalic typical for wastewater/coastal — confirm against supplier chemical-resistance data
GRIT TOPSlip performanceWet/oily service; supplier test data under a current method (e.g. DIN 51130 R-rating) on request — ASTM C1028 withdrawn
ASTM E84 CLASS 1Fire performanceInterior code compliance
UDL 4.8 kPa @ 1200 SPANLoad + span pairA load without span is unenforceable
Δ ≤ L/200Deflection limitThe checkable pass/fail criterion

Put the full specification in the drawing’s general notes (one grating paragraph) and use the short callout at each plan location; for projects with multiple grating zones, a grating schedule table (mark, depth, mesh, resin, span, zone) keeps plans clean.

Plan details that prevent field problems

Three drawing details do more for FRP grating performance than anything in the notes:

  • Bearing direction arrow. Pultruded grating carries load along its bearing bars only. Show the bearing direction with an arrow on plan; a panel installed rotated 90° to its span has effectively no rated capacity and will be discovered by how it feels underfoot.
  • Support detail. Follow the manufacturer’s installation requirements; show support width and fastening layout on drawings (40 mm+ bearing typical). Friction alone is not an attachment.
  • Openings and cut-outs. Show field-cut openings on plan with the note that cut edges be sealed with matching resin (an unsealed cut edge is where chemical attack starts). For molded grating add that panels may be cut without derating; for pultruded grating note that a cut perpendicular to bearing bars removes the continuous bar — openings wider than one mesh cell at a panel edge need a trimmer bar.

Common callout mistakes that get submittals rejected

  • Specifying depth alone (“38 mm FRP grating”) — no mesh, resin, span or deflection basis; every bidder prices a different product.
  • Copying a steel grating note and appending “FRP” — steel notes reference NAAMM load classes and metal-bar conventions that have no FRP equivalent.
  • Stating a load without a span, or a span without a deflection limit — nothing is verifiable.
  • Omitting the resin line in a corrosive atmosphere — the cheapest compliant-looking bid wins, and the panel erodes.
  • Forgetting the bearing direction arrow — a fabrication-perfect panel installed wrong is still a failure.
  • Requiring “fiberglass grating, Bunnings-style” or any retail reference on commercial drawings — retail mesh panels are molded consumer product without published load tables; a spec drawing must reference industrial-grade pultruded or molded grating with test data behind it.

FAQ

What is the standard specification for FRP grating?

There is no single codified standard for configuration-and-performance specification in general use the way metal bar grating has NAAMM; FRP grating is specified by configuration and performance: depth, mesh opening, bar construction (pultruded I-bar/rectangular or molded), resin system, top surface, fire class (ASTM E84 Class 1 or local equivalent), and a load–span–deflection triple (e.g. 4.8 kPa UDL at 1,200 mm span, deflection ≤ L/200) backed by the manufacturer’s panel test data.

What resin should I call out for FRP grating?

Isophthalic polyester is the default corrosion grade for wastewater, coastal and general chemical exposure. Move up to vinyl ester for severe acid or solvent service; use phenolic where offshore or fire-critical low-smoke requirements apply. Orthophthalic is acceptable only for indoor, non-chemical service — and should never be the silent default on a corrosive project.

How far can 38 mm FRP grating span?

Per Fibergrate guidance, 914–1,067 mm is typical for 38 mm molded grating at 2.4–3.1 kPa pedestrian load, with deflection ≤ the lesser of L/120 or 9.5 mm; 51 mm deep panels reach 1,219–1,372 mm. Depth alone never sets span — always confirm against the specific manufacturer’s published load table for the exact depth, mesh and bar type specified; spans in different suppliers’ tables do not transpose.

Is there a standard test for long-term (seven-day) deflection of FRP grating?

Not a widely published one, and this catches many buyers out. A common specification line asks for “certified test results verifying long-term deflection criteria for a seven-day duration test” — but there is no dominant industry test procedure for sustained-load deflection of FRP grating the way there is for short-term uniform load. In practice the requirement gets resolved between engineer and manufacturer case by case. When you write the callout, name the acceptance criteria yourself: span, uniform load, allowable mid-span sag at day 7, and test temperature. A manufacturer who cannot state how they will run the test cannot certify the result.

How do I specify FRP grating for intermittent high-temperature exposure?

State two temperatures, not one. Manufacturers typically guarantee a continuous-use temperature for the resin system; one reported project had grating guaranteed to 70°C continuous, with process upset conditions spiking to 160°C. If the callout only lists the upset temperature, every standard resin will be disqualified; if it only lists the continuous temperature, the first upset may deform the panels. Write both: continuous operating temperature with duration, plus maximum upset temperature and its expected duration and frequency. Then let the supplier match a resin system — isophthalic, vinyl ester or phenolic — to the pair, and ask for the basis of their temperature claim.

Looking Forward
Your Next Project!

\n \n \n \n \n \n \n \n
Scroll to Top
Get Quote WhatsApp